01On every production lot
| Property | Method | Why it is there |
|---|---|---|
| Hardness | Shore A, ASTM D2240 | The single fastest indicator that a batch was mixed correctly. |
| Tensile strength | ASTM D412 | Catches under-cure and filler errors that hardness alone misses. |
| Elongation at break | ASTM D412 | Together with tensile, defines the compound against its datasheet. |
| Compression set | ASTM D395, method B | The property that actually decides seal life at temperature. |
| Specific gravity | ASTM D297 | Detects loading errors and compound substitution. |
| Dimensions | Optical or contact, per drawing | ID, CS and OD against the tolerance band on the drawing. |


02What ships with the parts
Certificate of conformity
States the compound, the standard revision and the designations the parts were made to — including both the old and the current designation where one superseded the other.
Batch record
Compound batch, cure date and lot number, kept for seven years. That is what makes a traceability question answerable two years later.
Test report
The physical properties measured on the lot, against the compound datasheet. Available for any shipment on request, and quoted as standard on qualification lots.
Third-party testing
Where a customer's qualification requires an accredited laboratory, we send samples out and quote the cost with the parts. We do not issue certificates we are not entitled to issue.
03Standards we work to
Size dimensions follow AS568 for inch parts and ISO 3601-1 for metric parts. Surface acceptance follows ISO 3601-3 unless the drawing specifies otherwise. Material callouts follow the customer's drawing, or ASTM D2000 line callouts where the drawing cites them. Military designations are made to the document the designator names, where we can obtain that document.